Introduction |
Cold heading wire is mainly used for various kinds of fasteners and pins for construction & automotive use as well as precision disc use. It has excellent corrosion resistance and mechanical properties depending on the grades, In order to obtain good-shaped upsetting and threading,it is very essential to select the most suitable grades with highest quality. |
Product Grade |
Product Grade |
Chemical Composition (%) |
AISI |
SUS |
C |
Si |
Mn |
P |
S |
Ni |
Cr |
Other |
304 |
304 |
≤0.08 |
≤1.00 |
≤2.00 |
≤0.045 |
≤0.030 |
8.00-10.50 |
18.00-20.00 |
- |
302HQ |
XM-7 |
≤0.08 |
≤1.00 |
≤2.00 |
≤0.045 |
≤0.030 |
8.00-10.50 |
17.00-19.00 |
Cu:3.00-4.00 |
- |
(304J3) |
≤0.08 |
≤1.00 |
≤2.00 |
≤0.045 |
≤0.030 |
8.00-10.50 |
18.00-19.00 |
Cu:1.00-3.00 |
(305) |
305J1 |
≤0.08 |
≤1.00 |
≤2.00 |
≤0.045 |
≤0.030 |
11.00-13.50 |
16.50-19.00 |
- |
316 |
316 |
≤0.08 |
≤1.00 |
≤2.00 |
≤0.045 |
≤0.030 |
10.00-14.00 |
16.00-18.00 |
Mo:2.00-3.00 |
- |
- |
≤0.03 |
≤1.00 |
≤2.00 |
≤0.040 |
≤0.030 |
10.50-13.50 |
16.00-18.00 |
Cu:2.80-3.80 Mo:2.00-3.00 |
430 |
430 |
≤0.12 |
≤0.75 |
≤1.00 |
≤0.040 |
≤0.030 |
- |
16.00-18.00
|
|
(We can provide other grades subject to your special requirement.) |
Characteristics |
|
High formability Low working stress Excellent surface quality Most proper hardenability And low tool wearing Superior low magnetism After heading & threading | |
|
|
|
|